for applications with moderate cyclic fatigue requirements
Precipitation hardening for increased strength with maintained ductility during forming.
suitable for use in slightly elevated temperatures
Property | Value | ||
---|---|---|---|
E modulus of elasticity | Abt. 180 kN/mm2 in drawn condition. | Abt. 185 kN/mm2 after heat treatment. | |
G modulus of shear | Abt. 70 kN/mm2 in drawn condition. | Abt. 73 kN/mm2 after heat treatment. | Density: 7.90 kg/dm3. |
Nearest equivalent product standards | EN ISO 6931-1 | ASTM A313 | AMS 5678 F | JIS G4314 |
Nearest equivalent steel grades | EN/DIN 1.4568 | AISI/SAE 631 | JIS SUS 631 |